Docol® 800DP
A cold rolled steel for the front structure of your body in white
For Docol® 800 DP there is a big difference in yield and tensile strength in un-deformed areas. The work hardening in forming is very strong. With its lean composition these steels are easy to weld but sensitive to heat treatment (> 200 °C). Designed to meet EN10131.