Docol 800DL dual-phase steel combines excellent formability with high strength for safety in cars.
This steel undergoes special heat treatment in a continuous annealing line, producing a two-phase structure. Ferrite that imparts unique forming properties represents one phase, and martensite that accounts for the strength represents the other phase.