180 180
Docol 800CP
Docol products for automotive

Docol® 800CP

Hot rolled steel suitable for control arms and other parts in chassis

Docol® HR 800CP has good fatigue properties when it comes to low cycle fatigue and also offers better flanging and ISO hole expansion performance compared to DP grades. This grade is suitable for applications where high strength, good bendability and stretch-flange ability is required. One typical example is the lower control arm. Sub frames made from hot rolled, advanced high strength steel with excellent fatigue properties provide robustness as well as low weight. Designed to meet VDA 239-100:2016 and EN 10051 standards.

We supply many steel grades according to standards like EN, VDA and different OEM standards. If you don't find a specific standard in the table below, please contact your nearest SSAB representative for more detailed information.

Dimension Range

Cold rolled / UC: thickness 0.50-2.10 mm, width up to 1527 mm.

Cold rolled / GI, GA, ZA: thickness 0.80-2.50 mm, width up to 1460 mm.

Hot rolled / UC: thickness 2.00-4.00 mm, width up to 1500 mm.

Hot rolled / GI: thickness 2.00-3.50 mm, width up to 1400 mm.

Slit strip and cut to length sheets are available upon request.

Grade and coating specific restrictions on available dimensions may occur.

Available Standards

VDA 239-100:2016

SSAB

Docol 800CP

Docol 800CP

USED FOR
STANDARDS
DATA SHEET
USED FOR

Automotive

STANDARDS

VDA239-100:2016

SSAB

DATA SHEET