Docol 780DP

Steels that can contribute to car weight reduction

Our production-friendly Docol 780DP steels have good formability and weldability.

These steels undergoe special heat treatment in a continuous annealing line, producing a two-phase structure. Ferrite that imparts unique forming properties represents one phase, and martensite that accounts for the strength represents the other phase.

We supply many steel grades according to standards like EN, VDA and different OEM standards. If you don't find a specific standard in the table below, please contact your nearest SSAB representative for more detailed information.

Dimension range

Docol CR440Y780T-DP / UC: thickness 0.50-2.10 mm, width up to 1527 mm, length up to 8500 mm.

Docol CR440Y780T-DP / GI&GA: thickness 0.80-2.00 mm, width up to 1445 mm, length up to 6000 mm.

Docol CR440Y780T-DP / ZA: thickness 0.80-2.00 mm, width up to 1445 mm, length up to 6000 mm. (upon request)

Slitting to narrow coils and cutting to sheets are available upon request.

Available Standards

VDA 239-100:2016

EN 10131

EN 10143