180 180
Docol 700LA
Docol products for automotive

Docol® 700LA

Hot rolled structural steels

The Docol® 700LA steels are high-strength low-alloy steels that offer consistent properties for modern, rapid production methods.
The Docol® 700LA steels are made for cold forming of stronger and lighter structures.

Typical applications include components and parts in demanding load-bearing structures such as chassis.

Docol® HR700LA-UC can after agreement be adapted and delivered as dual certified with S700MC according to EN 10149-2:2010.

We supply many steel grades according to standards like EN, VDA and different OEM standards. If you don't find a specific standard in the table below, please contact your nearest SSAB representative for more detailed information.

Dimension Range

Hot rolled / UC: thickness 2.00-6.00 mm, width up to 1600 mm.

Hot rolled / EG: thickness 2.00-3.00 mm, width up to 1360 mm.

Hot rolled / GI: thickness 2.00-4.00 mm, width up to 1400 mm.

Slit strip and cut to length sheets are available upon request.

Grade and coating specific restrictions on available dimensions may occur.

Available Standards

VDA 239-100:2016

Docol 700LA

Docol 700LA

USED FOR
STANDARDS
DATA SHEET
USED FOR

Automotive

STANDARDS

VDA239-100:2016