Docol® 600LA
A hot-rolled steel made for cold forming
The Docol® 600LA is a high-strength low-alloy steel that offer consistent properties for modern, rapid production methods.
Typical applications include components and parts such as load-bearing structures, for example chassis.
Docol® HR600LA-UC can after agreement be adapted and delivered as dual certified with S600MC according to EN 10149-2:2010.