180
Ferritic Bainitic
Docol products for automotive

Docol® 600FB

Docol® 600FB

Docol® 600FB is a modern hot-rolled advanced high strength steel with a matrix of ferrite or strengthened ferrite containing bainite or strengthened bainite and with a refined grain size.

The steel grade is well suited for cold formed automotive components such as wheels, chassis components and different structural reinforcements. Formability is very good, especially in hole expansion.

Docol® HR440Y580T-FB meets the requirements of HR440Y580T-FB according to VDA 239-100.

Dimension Range

Hot rolled / UC: thickness 2.00-4.00 mm, width up to 1600 mm.

Slit strip and cut to length sheets are available upon request.

Available Standards

VDA 239-100:2016

Docol 600FB

Docol 600FB

USED FOR
DIMENSIONS
STANDARDS
DATA SHEET
USED FOR

Automotive

DIMENSIONS

T: 2 - 4 mm

W: Up to 1600 mm

STANDARDS

VDA239-100:2016

DATA SHEET