Docol 600CP
Docol products for automotive

Docol® 600CP

Hot-dip coated steel for lightweight vehicles

Docol® 600CP is a steel for complex shapes with energy absorbing capability and corrosion resistance.

Examples include complex body-in-white (BIW) and other automotive components. Galvanic corrosion protection of these zinc-based coated products makes them ideal for wet area components.

We supply many steel grades according to standards like EN, VDA and different OEM standards. If you don't find a specific standard in the table below, please contact your nearest SSAB representative for more detailed information.

Dimension Range

Cold rolled / GI, GA, ZA: thickness 0.70-2.50 mm, width up to 1520 mm.

Slit strip and cut to length sheets are available upon request.

Grade and coating specific restrictions on available dimensions may occur.

Available Standards