Docol 590DP

Dual-phase steel for automotive applications 

Docol 590DP dual-phase steels have good formability and weldability and are suitable for car safety components such as seat racks.

We supply many steel grades according to standards like EN, VDA and different OEM standards. If you don't find a specific standard in the table below, please contact your nearest SSAB representative for more detailed information.

Dimension range

Docol CR330Y590T-DP / UC: thickness  0.50-2.10 mm, width up to 1500 mm, length up to 8500 mm.

Docol CR340Y590T-DP / UC: thickness 0.50-2.10 mm, width up to 1500 mm, length up to 8500 mm.

Docol CR330Y590T-DP / GI: thickness 0.70-3.00 mm, width up to 1520 mm, length up to 6000 mm.

Docol CR330Y590T-DP / GA & ZA: thickness 0.70-2.50 mm, width up to 1520 mm, length up to 6000 mm.

Slitting to narrow coils and cutting to sheets are available upon request.

Available Standards

VDA 239-100:2016

EN 10338:2015

EN 10131

EN 10143

Docol 590DP

Docol 590DP