Docol® 550LA

Hot rolled high-strength low-alloy steels

The Docol® 550LA steels are high-strength low-alloy steels that offer consistent properties for modern, rapid production methods.

These steels are suitable for operations where higher strength is needed. It offers consistent properties for modern, rapid production methods. 

Typical applications include bent profiles.

Docol® HR550LA-UC can after agreement be adapted and delivered as dual certified with S550MC according to EN 10149-2:2010.

We supply many steel grades according to standards like EN, VDA and different OEM standards. If you don't find a specific standard in the table below, please contact your nearest SSAB representative for more detailed information.

Dimension Range

Hot rolled / UC: thickness 2.00-6.00 mm, width up to 1600 mm.

Hot rolled / GI: thickness 2.00-4.50 mm, width up to 1450 mm.

Slit strip and cut to length sheets are available upon request.

Grade and coating specific restrictions on available dimensions may occur.

Available Standards

VDA 239-100:2016

Docol 550LA

Docol 550LA

USED FOR
STANDARDS
DATA SHEET
USED FOR

Automotive

STANDARDS

VDA239-100:2016

DATA SHEET