Docol® 500DP
Steel for forming and welding automotive details
Docol® 500DP dual-phase steel possesses good formability and weldability and is suitable for car safety components such as reinforcements.
This steel undergoes special heat treatment in a continuous annealing line, producing a two-phase structure. Ferrite that imparts unique forming properties represents one phase, and martensite that accounts for the strength represents the other phase.