Docol 420LA
A high-strength steel for modern production
The Docol 420LA steels are high-strength low-alloy steels, available both as hot rolled and cold rolled.
These steels are suitable for operations where higher strength is needed. It offers consistent properties for modern, rapid production methods.
Docol HR420LA-UC can after agreement be adapted and delivered as dual certified with S420MC according to EN 10149-2:2010.