Docol 1180CP - our strongest CP steel for automotive applications

Docol 1180CP complex phase steel is developed for increased safety in cars.

Its ultra-high strength allows for weight reduction in BIW applications. This steel undergoes special heat treatment in a continuous annealing line, producing a complex phase structure.