180 180
Ramor 450

Ramor® 450

Combines ballistic properties with impact toughness.

Ramor® 450 is a medium-hard protection plate combining ballistic properties with impact toughness, at 8‑16 mm (0.315‑0.630″) thick and 400‑480 HBW.

Ramor® 450 is not intended for further heat treatment. Read more on SSAB armor and ballistic steels.

Dimension Range

Ramor 450 is available as plate in thickness between 8.0 - 16.0 mm.

Available Standards

EN 10029

Ramor 450

Ramor 450

USED FOR
DIMENSIONS
STANDARDS
DATA SHEET
USED FOR

Armored

DIMENSIONS

T: 8 - 16 mm

STANDARDS

EN 10029

DATA SHEET