Customer story

AA Diesel Truck Bodies gains 10-plus years of product life for end users with Hardox® wear plate

For 20 years, family company AA Diesel Truck Bodies has supplied custom-made truck bodies to the demanding Australian transport industry. The right steel in the body units will help the end user to reduce weight by 10 to 20 percent and increase the payload.

Life can be hard on truck bodies. Especially if you are transporting big rocks, metal or other heavy or rough materials. Alija Siskovic, founder of the company AA Diesel Truck Bodies, knows this well. Using the right steel in the truck bodies can translate into 10-plus years of product life for the end user.


Customers are happy to order truck bodies made of Hardox® steel 

The company used to make its truck bodies from 350-grade steel. Although a high-tensile steel, it saw a lot of wear and tear and damage, and ultimately the bodies wouldn’t last. AA Diesel Truck Bodies started looking for somebody who could deliver more durable steel. This led them to SSAB and Hardox® wear plate.

“We started using Hardox wear plate because Australian people, who use tippers and trucks that experience hard work to the body, have noticed that it’s the best material,” Alija Siskovic says.

“People are pleased. They ask us which material we use for the body, and as soon as we say that it’s Hardox from SSAB, they’re happy to order.”

Alija Siskovic, AA Diesel Truck Bodies founder

He points out that Hardox® wear plate is good for everything, including welding. “People are pleased. They ask us which material we use for the body, and as soon as we say that it’s Hardox from SSAB, they’re happy to order.”


Hardox® 500 Tuf seen as an excellent product

Arnel Siskovic, Alija’s son, and today the company’s managing director, adds: “We've experimented with Hardox 500 Tuf, and that’s also an excellent product. But generally, Hardox 450 steel is our main material.” 

He estimates that you could easily get 10 years extra using a Hardox® steel body compared with a 350-grade steel body. “Hardox steel bodies are generally more expensive,” he says. “But when you take their longevity into account, we get so many orders that we have a huge amount of work, because people know that it’s money well spent.”

By using a Hardox® product in the truck body, Arnel Siskovic explains, you can go from an eight-millimeter plate to six millimeters in the floor, and from a six-millimeter plate to five millimeters in the sides. “You’re gaining a lot because you’re saving on weight, probably 10 to 20 percent. Your payload is higher in combination with the longevity of the body. So there are many positives in using this product.”

The future demands better-quality steel 

Arnel’s younger sister Amina Siskovic works as office manager at the family company while studying mechanical engineering at a university. She sees lighter material as the future of the industry. “After my exam I'll come back here and help improve new products,” she says. “As the industry moves into a new phase of electric trucks and autonomous vehicles, we need to develop trucks that are lighter, safer and more efficient. To do that, we need to use better-quality materials, which is why we use Hardox steel.”

SSAB suggested that AA Diesel Truck Bodies should become a Hardox® In My Body customer program member. “We were buying a lot of steel,” Arnel Siskovic says. “I didn’t know too much about this membership. But I said, if it’s a sign of quality, then it surely can help my business.”

And indeed it has. “Truck drivers know now when they see the sticker that it’s a quality body, that it’s an endorsed body builder,” Arnel Siskovic says. “They know that they’re getting the best.”


What is the impact of being a Hardox® In My Body member on secondhand value?

“There is a higher value in secondhand truck bodies with Hardox wear plate,” Arnel Siskovic says. “AA Diesel Truck Bodies has got trucks that have had Hardox steel bodies for five or six years. The paint might have a few scratches here and there, but the structural part is intact. It’s still very straight, with no dents, no damage, and the floor is still very flat, ready to continue carrying big loads.

“We’re very proud to be a Hardox In My Body member,” he says. “It’s helped us grow our business. I like the peace of mind it gives my customers, and using the Hardox product also gives me peace of mind that I’m selling the best that I can sell. It’s set us apart from the competition because it’s a sign of quality.”

 

About AA Diesel Truck Bodies

  • Based in Doveton, Victoria, in Australia
  • Family business, founded in 1996
  • Delivering custom-made truck bodies all over the country
  • Products include buckets, bodies and various attachments

 

www.aadieseltruckbodies.com.au

SSAB steel used by AA Diesel Truck Bodies

  • Most truck bodies made from Hardox® 450  wear plate, generally five millimeters in the sides and six millimeters in the floor
  • Hardox® 500 Tuf  wear plate

Contact us

No matter where you are located, we have local support that can answer your questions.

Sign up for newsletters

Visit our subscription center to manage all your SSAB newsletters subscriptions

Don't miss out!

Hardox® wear plate

Hardox® wear plate is the world's leading abrasion-resistant (AR) steel. Hardox® is hard through and through, from the surface deep down to its core, giving you extended service life and high productivity in the most challenging environments.

Hardox® In My Body

Look for the Hardox® In My Body branded sign if you’re looking for bodies that are hard, tough, cost efficient and made from genuine Hardox® wear plate.

Related articles

Apr 28 2020

Farmtech’s agricultural tippers made from Hardox® steel are “indestructible,” according to customers

In the midst of the beautiful Slovenian countryside, tipper body specialist Farmtech constructs high-quality equipment for the demanding agricultural industry, which runs continuous transports with heavy loads. The recipe for the success of the heavy-duty dump tipper Gravis 2000 is to use Hardox® 450 wear plate throughout the model’s body.

Mar 25 2020

Betonstar reaches higher with lighter weight through Strenx® steel

Concrete pumps used in the construction of tall buildings need a boom structure that is strong and reliable while also striving for light weight. Turkish Betonstar has met these requirements by using only Strenx® performance steel throughout its structures. The result is longer, stronger and lighter products.

Feb 25 2020

By incorporating Hardox® and Strenx® steels in tippers, Fesan makes sure not to compromise on quality

Turkish trailer and tipper manufacturer Fesan Makina’s key driver is customer satisfaction. When customers asked for stronger and lighter equipment, that is what they got, as Fesan switched to Hardox® wear plate and Strenx® performance steel. By including this and other innovative features in the new tipper model, the company is keeping its position as a market leader.

180