    General Product Description

    SSAB M43 is a micro-alloyed steel grade for quench hardening. Its fine-grain micro-structure allows critical workshop operations without risk for micro-cracking. The self-tempering properties prevent formation of hardening cracks. The degree of hardness and toughness that can be achieved after heat-treatment will provide end products with a wear- and shock resistance ratio that ensures longer lifetime.

    Dimension Range

    Hide/Show specific columns Edit
    Select columns to display
      Delivery form Thickness
      (mm)
      Width
      (mm)
      Length
      (mm)
      Hot rolled coil 3.0 - 12.0 1) 870 - 1800
      Hot rolled slit coil 3.0 - 12.0 1) 100 - 755
      Hot rolled sheet 3.0 - 12.0 1) 1000 - 1800 - 13000
      Compare parameters

      Select one parameter to compare

      Comparison

        1) Please check thickness/width combinations available.

        Mechanical Properties (typical values)

        Hide/Show specific columns Edit
        Select columns to display
          Product type Typical yield strength Rp0.2 (MPa) Typical tensile strength Rm (MPa) Typical Elongation A (%),
          not guaranteed
          Typical Hardness
          (HRC), not guaranteed
          As rolled 440 660 16 18
          Water quenched 2400 58
          Water quenched and tempered (175° C) 56
          Oil quenched 1750 52
          Oil quenched and tempered (175° C) 51
          Compare parameters

          Select one parameter to compare

          Comparison

            Bending radius

            For further information, please consult your local SSAB contact person or contact SSAB’s Technical Customer Service.

            Material Testing

            A material test certificate Type 2.2 according to EN 10204 (chemical composition) is part of the delivery. A material test certificate according Type 3.1 according to EN 10204 (mechanical properties) can be provided by special agreement.

            Impact Properties (typical values)

            Hide/Show specific columns Edit
            Select columns to display
              Product condition Longitudinal test, typical impact energy,
              Charpy V 10x10 mm test specimen
              As rolled / 20.0 °C
              Water quenched 25 J / 20.0 °C
              Water quenched and tempered (175° C) 37 J / 20.0 °C
              Oil quenched 38 J / 20.0 °C
              Oil quenched and tempered (175° C) 39 J / 20.0 °C
              Compare parameters

              Select one parameter to compare

              Comparison

                Product condition
                As rolled
                Longitudinal test, typical impact energy,
                Charpy V 10x10 mm test specimen
                / 20.0 °C
                Product condition
                Water quenched
                Longitudinal test, typical impact energy,
                Charpy V 10x10 mm test specimen
                25 J / 20.0 °C
                Product condition
                Water quenched and tempered (175° C)
                Longitudinal test, typical impact energy,
                Charpy V 10x10 mm test specimen
                37 J / 20.0 °C
                Product condition
                Oil quenched
                Longitudinal test, typical impact energy,
                Charpy V 10x10 mm test specimen
                38 J / 20.0 °C
                Product condition
                Oil quenched and tempered (175° C)
                Longitudinal test, typical impact energy,
                Charpy V 10x10 mm test specimen
                39 J / 20.0 °C

                Chemical Composition (ladle analysis)

                Hide/Show specific columns Edit
                Select columns to display
                  C
                  (%)
                  Si
                  (%)
                  Mn
                  (%)
                  S
                  (max %)
                  P
                  (max %)
                  Cr
                  (max %)
                  0.39 - 0.47 0.13 - 0.23 0.20 - 0.30 0.010 0.020 0.10
                  Compare parameters

                  Select one parameter to compare

                  Comparison

                    SSAB M43 is micro-alloyed with Nb, Ti and V.

                    Carbon Equivalent

                    Hide/Show specific columns Edit
                    Select columns to display
                      Delivery form Hot rolled strip
                      Typical CET (%) 0.53
                      Compare parameters

                      Select one parameter to compare

                      Comparison

                        Delivery form
                        Typical CET (%)
                        Hot rolled strip
                        0.53
                        CET and CEV formula

                        Tolerances

                        SSAB M43 is delivered with SSAB tolerances, which meet and exceed the requirements in EN 10051. Tighter tolerances are available upon request

                        Thickness

                        2/3 of EN 10051.

                        Width

                        Hot rolled coil: -0/+20mm (trimmed edges -0/+2 mm).

                        Hot rolled slit coil: -0/+1mm.

                        Hot rolled sheet: -0/+20mm (trimmed edges -0/+2 mm).

                        Length

                        -0/+20mm (only available for cut to length sheets).

                        Shape

                        According to EN 10051.

                        Flatness

                        ≤ 6 mm/1 m ruler deviation (only valid for cut to length sheets).

                        Surface Properties

                        According to EN 10163-2 Class A, Subclass 3.

                        Delivery Conditions

                        Hot rolled coils, slit coils and sheet are delivered in as rolled (+AR) condition.

                        Surface Condition

                        Hot rolled coil products are available in non-pickled, pickled dry or pickled & oiled condition.

                        Fabrication and Other Recommendations

                        For information concerning fabrication, see SSAB´s brochures on www.ssab.com or consult Tech Support.

                        Appropriate health and safety precautions must be taken when bending, welding, cutting, grinding or otherwise working on the products.

                        Contact Information

                        www.ssab.com/contact