Strenx_tubes_top-banner
Strenx_tubes_top-banner

Jajaran produk Strenx® Tube

Jajaran tubes Strenx® berbentuk circular, square, dan rectangular – bahkan bentuk kustom dapat disediakan atas permintaan. Strenx® tubes memiliki rasio strength to weight yang lebih tinggi untuk equipment kelas berat.

Order trial material Get technical advice

Suitable applications

Advanced load-bearing structures in transportation, lifting and agriculture

Product types

High-strength hollow sections

Available shapes

Circular, square and rectangular

High-strength steel grades for high-performing structural applications

Strenx® Tube 700MLH

Typical applications for Strenx® Tube 700MLH include load-bearing structures in lifting, material handling, transportation and agriculture, especially in conditions that require extremely high toughness.

Strenx® Tube 900MH

Typical applications for Strenx® Tube 900MH include advanced load-bearing structures in the lifting, transportation and agriculture segments.

Strenx® Tube 960MH

Typical applications for Strenx® Tube 960MH include advanced load-bearing structures in the lifting, transportation and agriculture segments.

Strenx® Tube 700QLH

Typical applications for Strenx® Tube 700QLH are load-bearing lattice structures in lifting, material handling, transportation and agriculture, especially in conditions where high toughness is needed.

Strenx® Tube 960QLH

Typical applications for Strenx® Tube 960QLH are load-bearing lattice structures in lifting, material handling, transportation and agriculture, especially in conditions where high toughness is needed.

Driving performance with My Inner Strenx® planting and seeding machine by Equalizer

Equalizer lightens the load in farming

“Our customers got a 40% lighter row planter when we upgraded to Strenx® high-strength 
structural steel,” sasys Gideon Schreuder, Managing Director at Equalizer

Made for predictable performance in the workshop

Welding

Welding

Strenx® tubes can be welded using any conventional welding method. MAG welding is the most common technique today, since it is very easy to automate for high productivity.

Machining

Strenx® tubes can usually be machined without special equipment. Stable machinery fitted with high-speed steel and carbide tools is recommended when drilling, countersinking, tapping, and milling.
Thermal cutting

Thermal cutting

The properties and fine surface finish of Strenx® tubes make it perfect for laser cutting. Strenx Tubes can also be thermal-cut with oxy-fuel flame and plasma. Since tubes are cold formed, they contain residual stresses. Proper design can control distortion when cutting. If distortion becomes a problem the tubes can be stress relief annealed.

	Mechanical cutting

Mechanical cutting

Strenx® Tubes can be sawed with the usual cutting tools. Compared with mild steel tubes, saw blade wear can be lower, since the low carbon equivalent prevents the longitudinal weld seam from hardening during welding.

	Strenx guarantees

Strenx® guarantees

Strenx® Tubes and Sections meet or exceed the tolerances of European standards: EN10219 for cold formed welded steel structural hollow sections and EN10210 for hot finished steel structural hollow sections.

Strenx® Tube products

 
PRODUCT NAME DIMENSIONS  STANDARDS 
STRENX® TUBE 700MLH

Thickness 2.0 - 10.0 mm
Diameter: 48.3 - 323.9 mm
Width: 40 - 300 mm
Mill length: 6000 - 12000/18000 mm

 EN 10219-3
 
STRENX® TUBE 900MH  Thickness 4.0 - 6.0 mm
Diameter: 139.7 - 244.5 mm
Width: 100 - 200 mm
Mill length: 6000 - 12000/18000 mm
EN 10219-3
STRENX® TUBE 960MH  Thickness 4.0 - 6.0 mm
Diameter: 139.7 - 244.5 mm
Width: 100 - 200 mm
Mill length: 6000 - 12000/18000 mm
EN 10219-3
STRENX® TUBE 700QLH Thickness 3.0 - 6.0 mm
Diameter: 76.1 - 133.0 mm
Mill length: 6000 - 12000 mm
EN 10210
STRENX® TUBE 960QLH

Thickness 3.0 - 6.0 mm
Mill length: 6000 - 12000 mm

EN 10210-2

Download brochure

pdf 362 Kb
Strenx® Tubes leaflet

Hubungi Kami

Inquiry Anda

Informasi kontak Anda

* Wajib diisi

Apa yang dapat kami bantu?

Lihat kebijakan privasi SSAB untuk informasi lebih lengkap tentang cara kami memproses data pribadi