The size of the joint root gap

The width of the root gap affects the penetration of the first weld pass.

In other words, a consistent width of the root gap supports a high quality of the welded joints, including further resistance to lack of root penetration. Another reason to have relatively small root gaps is that this measure supports a higher resistance to hydrogen cracks and lowered distortions in the structure. The maximum size of the root gap is set to 3 mm to support a high resistance to hydrogen cracks.

b: max 3 mm

Contact Technical support


The information in this report is only applicable to SSAB’s products and should not be applied to any other products than original SSAB products. 


This report provides general results and recommendations for SSAB steel products. This report is subject to SSAB’s Terms of Use. It shall be the user's responsibility to verify that the information contained herein is correct and is suitable to be used for the particular purpose and application of the user. The report is intended to be used by professional users only who possess adequate expertise, qualification and knowledge for the safe and correct use of the results and recommendations in this report. This report is provided “as is”. The use of the report is at user’s own discretion and risk and that users will be solely responsible for any use of this report. SSAB disclaims any liability for the content or potential errors of this report, including but not limited to warranties and condition of merchantability or fitness for a particular purpose or suitability for individual applications. SSAB shall not be liable for any kind of direct or indirect damages and/or costs related to or arising therefrom, whether special, incidental, consequential or directly or indirectly related to the use of, or the inability to use, the report or the content, information or results included therein.