How to weld > Joint preparations > Joint methods

Joint methods

A sound welded joint requires proper joint preparation both before and during the welding process. Accurately preparing the joint will also help to prevent various types of welding defects.

There are several methods that can be applied for joint preparation. Those methods are the same for joint preparations of all unalloyed and low-alloyed steels as for the Hardox® and Strenx® grades. The most common preparation methods are thermal cutting, milling and grinding. In addition, shearing and punching can be used, however their usage is limited to the Strenx® grades and for Hardox® grades with hardness values up to 450 HBW.

If thermal cutting is used, a thin oxide or nitride layer will be present that is approximately up to 0.2 mm (0.008”) thick. These layers are removed before welding, usually by grinding.

Suitable recommendations for thermal cutting can be found in How to cut and the machining recommendations in How to machine.

Contact Technical support


The information in this report is only applicable to SSAB’s products and should not be applied to any other products than original SSAB products. 


This report provides general results and recommendations for SSAB steel products. This report is subject to SSAB’s Terms of Use. It shall be the user's responsibility to verify that the information contained herein is correct and is suitable to be used for the particular purpose and application of the user. The report is intended to be used by professional users only who possess adequate expertise, qualification and knowledge for the safe and correct use of the results and recommendations in this report. This report is provided “as is”. The use of the report is at user’s own discretion and risk and that users will be solely responsible for any use of this report. SSAB disclaims any liability for the content or potential errors of this report, including but not limited to warranties and condition of merchantability or fitness for a particular purpose or suitability for individual applications. SSAB shall not be liable for any kind of direct or indirect damages and/or costs related to or arising therefrom, whether special, incidental, consequential or directly or indirectly related to the use of, or the inability to use, the report or the content, information or results included therein.