To minimize the risk of hydrogen cracking, follow these recommendations:
  • Preheat the weld area to the recommended minimum temperature.
  • Measure the preheat temperature according to preheating recommendations.
  • Use processes and consumables that provide a maximum hydrogen content of 5 ml/100 g weld metal.
  • Keep the joint clear from impurities like rust, grease, oil, or frost.
  • Use only classifications for welding consumables recommended by SSAB.
  • Apply a proper welding sequence to minimize residual stresses.
  • Place weld starts and stops preferably at least 50–100 mm (2”–4”) from a corner to avoid excessive stresses in these regions, see illustration below.
  • Avoid a root opening size exceeding 3 mm (1/8”); see illustration below.
  • Gap size should not exceed 3 mm (1/8”); see illustration below.

Avoid start and stop in highly stresses areas and root gaps larger than 3 mm.

Contact Technical support


The information in this report is only applicable to SSAB’s products and should not be applied to any other products than original SSAB products. 


This report provides general results and recommendations for SSAB steel products. This report is subject to SSAB’s Terms of Use. It shall be the user's responsibility to verify that the information contained herein is correct and is suitable to be used for the particular purpose and application of the user. The report is intended to be used by professional users only who possess adequate expertise, qualification and knowledge for the safe and correct use of the results and recommendations in this report. This report is provided “as is”. The use of the report is at user’s own discretion and risk and that users will be solely responsible for any use of this report. SSAB disclaims any liability for the content or potential errors of this report, including but not limited to warranties and condition of merchantability or fitness for a particular purpose or suitability for individual applications. SSAB shall not be liable for any kind of direct or indirect damages and/or costs related to or arising therefrom, whether special, incidental, consequential or directly or indirectly related to the use of, or the inability to use, the report or the content, information or results included therein.