How to cut > How to get high edge quality with oxy fuel cutting of steel

How to get high edge quality with oxy-fuel cutting of steel

The photos below shows various scenarios of cutting edge quality along with corresponding improvement suggestions. These examples help identify optimal cutting conditions and highlight common issues encountered during cutting operations.

Optimal cutting edge quality

Too low oxygen cutting pressure

Too low heat input

Too high heat input

Nozzle to plate distance too close

Nozzle to plate distance too far

Too high cutting speed

Too low cutting speed

Low cutting speed combined with low cutting oxygen pressure, resulting in a wider kerf with potential slag inclusion.

Low cutting speed with insufficient cutting oxygen pressure, leading to an uneven cut surface and possibly increased dross.

Contact Technical support


The information in this report is only applicable to SSAB’s products and should not be applied to any other products than original SSAB products. 


This report provides general results and recommendations for SSAB steel products. This report is subject to SSAB’s Terms of Use. It shall be the user's responsibility to verify that the information contained herein is correct and is suitable to be used for the particular purpose and application of the user. The report is intended to be used by professional users only who possess adequate expertise, qualification and knowledge for the safe and correct use of the results and recommendations in this report. This report is provided “as is”. The use of the report is at user’s own discretion and risk and that users will be solely responsible for any use of this report. SSAB disclaims any liability for the content or potential errors of this report, including but not limited to warranties and condition of merchantability or fitness for a particular purpose or suitability for individual applications. SSAB shall not be liable for any kind of direct or indirect damages and/or costs related to or arising therefrom, whether special, incidental, consequential or directly or indirectly related to the use of, or the inability to use, the report or the content, information or results included therein.