Docol Tube 600LA

Docol® Tube 600LA

Provides a combination of high strength and formability

Docol® Tube 600LA is a modern high-strength low-alloy precision tube with hot rolled pickled surface condition. Available in circular, rectangular and square shapes. Customized shapes and other tailoring options are available upon request. Typically used in automotive industry, where durability, lightness and consistent properties are important.

Docol® Tube 600LA is manufactured by cold forming and high-frequency welding from clean, high-quality SSAB steel by modern and efficient tube lines.

Dimension Range

Docol Tube 600LA is available at circular, square and rectangular shapes. 

   
Circular 22 - 88.9 mm 
Square 30x30 - 60x60 mm 
Rectangular 30x20 - 100x40 mm 
Wall thickness 2.0 - 3.0 mm
Mill length 6000 mm

Other shapes, sizes and lengths are available upon request.

Available Standards

EN 10305-3

EN 10305-5