Strenx® 960 Plus is a structural steel that guarantees a minimum yield strength of 960 MPa.

Strenx® 960 Plus meets the requirements of EN 10 025-6 for the S960QL grade. Typical applications include demanding load-bearing structures.

Benefits include:

• Exceptional consistency within a sheet guaranteed by close tolerances
• High impact toughness which provides for good resistance to fractures
• Superior bendability and surface quality
• Weldability with excellent HAZ strength and toughness

Dimension Range

Strenx® 960 Plus is available as cut to length sheets in thicknesses of 2.0 - 8.0 mm. Strenx 960 Plus is available in widths up to 1600 mm and lengths up to 16000 mm depending on thickness. Please contact your sales representative for more information regarding dimensions.

 

Available Standards

EN 10025-6

EN 10051

EN 10163-2

Strenx rear underrun protection device

STRENX® 960 FOR STRONGER AND SAFER REAR UNDERRUN PROTECTION DEVICE

When quality matters, turning to Strenx® 960 high-strength steel for protection in your heavy-duty vehicles is a good choice. It is ideal in applications like rear underrun protection devices (RUPD), which help lower the risk of fatal injuries in rear-end collisions involving heavy-duty vehicles.

Strenx® 960 Plus

Strenx® 960 Plus

USED FOR
DIMENSIONS
STANDARDS
DATA SHEET
USED FOR

Structural

DIMENSIONS

T: 2 - 8 mm

W: Up to 1600 mm

L: Up to 16000 mm

STANDARDS

EN 10025-6

EN 10051

EN 10163-2