Polyester

Download data sheet

Select Language

Get datasheet by email
Close

Get datasheet by email

    General Product Description

    Polyester color coated steel from SSAB offers a wide range of colors inspired by Nordic nature. The typical gloss level is regular gloss, but other glosses are available from request.

    Product is typically used in profiled applications such as warehouses, agricultural buildings, halls and sheds. Polyester possesses good weather resistance properties (RC3) with a smooth surface. Polyester also offers a good flexibility when processing.

    The reverse side of the sheet is painted with a two-layer grey backside coating.

    Polyester complies with current REACH regulations and is fully free of chromates.

    SSAB’s color coated steels are all manufactured according to EN 10169.

    Technical Properties

    Hide/Show specific columns Edit
    Select columns to display
      Technical Properties Regular
      Gloss 35
      Minimum inner bending radius 3 x sheet thickness
      Scratch resistance 20 N
      UV radiation resistance RUV2-3
      Corrosion resistance 1) RC3
      Stain resistance Satisfactory
      Highest operating temperature 90 °C
      Fire classification, EN 13501-1 A1 s1 d0
      Coating thickness, nominal (primer + top coat) 25 µm
      Coating structure Smooth
      Steel designation 2) S280GD - S350GD, DX51D
      Zinc coating 275 g/m2
      Min steel thickness 2) 0.42 mm
      Steel width 2) 1000 - 1500 mm
      Compare parameters

      Select one parameter to compare

      Comparison

        Technical Properties
        Gloss
        Regular
        35
        Technical Properties
        Minimum inner bending radius
        Regular
        3 x sheet thickness
        Technical Properties
        Scratch resistance
        Regular
        20 N
        Technical Properties
        UV radiation resistance
        Regular
        RUV2-3
        Technical Properties
        Corrosion resistance 1)
        Regular
        RC3
        Technical Properties
        Stain resistance
        Regular
        Satisfactory
        Technical Properties
        Highest operating temperature
        Regular
        90 °C
        Technical Properties
        Fire classification, EN 13501-1
        Regular
        A1 s1 d0
        Technical Properties
        Coating thickness, nominal (primer + top coat)
        Regular
        25 µm
        Technical Properties
        Coating structure
        Regular
        Smooth
        Technical Properties
        Steel designation 2)
        Regular
        S280GD - S350GD, DX51D
        Technical Properties
        Zinc coating
        Regular
        275 g/m2
        Technical Properties
        Min steel thickness 2)
        Regular
        0.42 mm
        Technical Properties
        Steel width 2)
        Regular
        1000 - 1500 mm

        1) Classification into corrosion resistance categories is based on blistering, delamination and damage on bend of the coating after two years exposure in natural outdoor testing sites as specified in EN 10169.

        2) Maximum steel thickness is 1.5 mm and maximum steel width depends on steel thickness. For other steel dimensions or steel grades please contact SSAB Tech Support.

        Colors

        Below are the colors currently available. Other colors can be agreed upon separately.

        Colors shown in the color table are only indicative. To see the real visual appearance of the product, please order a color sample. Please note also that the same colors between the products may differ.

        35 Available Colors
        Preview colors
        Close

        Colors

        Polyester

        Frost White

        RR106 / SS0009

        Regular

        Nordic White

        RR1H3 / SS0020

        Regular

        Winter White

        RR20 / SS0005

        Regular

        White

        RR--- / SS0010

        Regular

        White

        RR135 / SS0248

        Regular

        White

        RR1G5 / SS0109

        Regular

        White

        RR1G6 / SS----

        Regular

        Fog White

        RR143 / SS----

        Regular

        White

        RR1L4 / SS0078

        Regular

        Limestone Grey

        RR268 / SS0022

        Regular

        Cloud Grey

        RR2B1 / SS----

        Regular

        Pebble Grey

        RR21 / SS0011

        Regular

        Stone Grey

        RR22 / SS0554

        Regular

        Rock Grey

        RR237 / SS0061

        Regular

        Grey

        RR2J9 / SS5036

        Regular

        Anthracite Grey

        RR2H8 / SS0087

        Regular

        Mountain Grey

        RR23 / SS0036

        Regular

        Ridge Grey

        RR2F7 / SS0035

        Regular

        Cliff Grey

        RR288 / SS0455

        Regular

        Slate Grey

        RR2H3 / SS0534

        Regular

        Nordic Night Black

        RR33 / SS0015

        Regular

        Walnut Brown

        RR32 / SS0387

        Regular

        Chestnut Brown

        RR887 / SS0435

        Regular

        Acorn Brown

        RR827 / SS0434

        Regular

        Cottage Red

        RR29 / SS0758

        Regular

        Tile Red

        RR750 / SS0760

        Regular

        Brick Red

        RR7F2 / SS0742

        Regular

        Red

        RR786 / SS5415

        Regular

        Harvest Yellow

        RR24 / SS0189

        Regular

        Silver Fir Green

        RR5J3 / SS0975

        Regular

        Leaf Green

        RR594 / SS0874

        Regular

        Pine Green

        RR11 / SS0830

        Regular

        Lake Blue

        RR35 / SS0558

        Regular

        Metallic Silver

        RR40 / SS0045

        Regular

        Metallic

        RR947 / SS----

        Regular

        Note for Metallic colors: To ensure tonal consistency of colors on a single exterior face, all material must come from the same production batch. Also the directionality of surfaces has to be consistent especially when sheets are cut to size.

        Reverse Side Coating

        Unless otherwise specified, the reverse side of the sheet is painted with a two-layer coating to further improve the corrosion resistance of the end product. The coating provides good adhesion properties to many adhesives and foams; nevertheless the compatibility needs to be tested case-specifically.

        Hide/Show specific columns Edit
        Select columns to display
          Technical Properties
          Nominal Coating Thickness (primer + top coat) 12 µm
          Color Grey
          Corrosion Resistance Min CPI3
          Compare parameters

          Select one parameter to compare

          Comparison

            Technical Properties
            Nominal Coating Thickness (primer + top coat)
            12 µm
            Technical Properties
            Color
            Grey
            Technical Properties
            Corrosion Resistance
            Min CPI3

            For easy material identification the reverse side of the sheet is stamped with the SSAB logo and the product name. The production year is marked to ease material traceability and can be referred to within the guarantee period. An arrow shows the direction of production to ensure installation in a uniform direction.

            Double Sided Products

            Polyester is also available as a double sided product. However, different sides of the sheet cannot be mixed due to the possibility of a visual difference. The reverse side may show wider variation in color and gloss.

            Protective Film

            Temporary protective films are available for protection during processing and installation. Protective films are applied on the top side of the Product. Films will be centered to the strip meaning that typically there are small unprotected areas in both edges of the strip. Unprotected area may be cut away if customer so wishes. Joined film strip ends are marked with red tape on the edge of the product.

            Products with protective film should be stored in dry and warm conditions, since the adhesion between protective film and color coating decreases both in high and low temperatures. Humidity changes also the adhesion properties and in worst case leaves the adhesive part of the film on the product surface.

            Adhesion of protective film increases over time, eventually making it difficult to remove the film from the Product’s surface. Due to that, protective film is recommended to be removed from the material as soon as possible, but no later than six months from the manufacturing of the Product or after one month from the end product installation depending on which comes first.

            Protective film decreases friction between coil windings, which creates a high risk of coil collapsing on thin gauge coils. Due to the risk of collapsing, SSAB does not recommend protective films for steel nominal thickness ≤ 0,60 mm. If protective film is essential, following precautions must be taken to minimize the risk of collapsing: Max coil weight < 5 tons and self-supporting coil protection shields must be used in the package.

            Typical protective film thickness is around 45µm, max working temperature +80°C and max and min stripping temperatures +40°C & -10°C.

            Protective film has a good resistance to forming but is susceptible to cuts. When working with material with a protective film, clean tools that do not damage the film, and appropriate methods are to be used. Cutting fluids are not needed because the film protects the material surface and reduces friction. Cutting fluids may also have negative impact on the protective film and its adhesion.

            Protective films can be recycled as plastics, combusted or disposed via the municipal waste management system depending on the local waste management guidelines and regulations.