SSAB Domex Tube 460MH Strenx 700QLH- high-strength steel tubing
The high-strength steel tubing at 700 MPa

Strenx® Tube 700QLH

Advanced high-strength structural hollow sections

Strenx® Tube 700QLH is plasma-welded, quenched and tempered hollow section with a minimum yield strength of 700 MPa.

Its high strength, combined with naturally stiff form of the welded hollow section, enables construction of stronger and lighter structures. Strenx® Tube 700QLH meets or exceeds the requirements of prEN 10210 (2016).

Typical applications are load-bearing lattice structures in the lifting, material handling and transportation sectors, especially in conditions where extremely good toughness is needed.

Dimension Range

Strenx® Tube 700QLH is available at circular shape.

   
Circular 76.1 - 133.0 mm 
Wall thickness 3.0 - 6.0 mm
Mill length 6000 - 12 000 mm

Available Standards

EN 10210-2