Commercial steel

ASTM A945

ASTM A945 GRADE 65 IS AVAILABLE BY INQUIRY ONLY.  ASTM A945 Grade 65 steel plate is a high-strength low-alloy structural steel with improved weldabilitiy, formability, and toughness for the use in the construction of naval ships.  ASTM allows the manufacturer the option to provide plates in thicknesses of 1.25 inches and less in the delivery conditions of as-rolled, normalized, or quenched and tempered.  SSAB's First Article Inspection report is available upon request. 
PRODUCT NAME
USED FOR
DIMENSIONS
DATA SHEET
PRODUCT NAME
ASTM A945 Grade 65
USED FOR

Structural

DIMENSIONS

T: 0.375 - 2 Inches

W: Up to 96 Inches

L: Up to 1080 Inches

DATA SHEET

English