ASTM A612
Commercial steel

ASTM A612

ASTM A612 specification is the Standard Specification for Pressure Vessel Plates, Carbon Steel, High Strength, for Moderate and Lower Temperature Service. ASTM A612 encompasses carbon-manganese-silicon steel plates intended for use in welded pressure vessels for moderate and low temperature service.

A612

A612

USED FOR
DIMENSIONS
DATA SHEET
USED FOR

Pressure Vessel

DIMENSIONS

T: 0.375 - 1 Inches

W: Up to 120 Inches

L: Up to 1020 Inches

DATA SHEET