Strenx® 110 XF
The thermomechanically rolled steel for cold forming
Strenx® 110 XF is a thermomechanically rolled steel at 110 ksi made for cold forming and used for light and heavy transportation components and solutions. It comes in coils, slit coils and cut-to-length sheets.
Thickness measurements in inches can be found in the data sheet.