Docol 500LA HSLA automotive steel

Docol® 500LA

For operations that require higher strength

The Docol® 500LA steels are high-strength low-alloy steels that offer consistent properties for modern, rapid production methods.

Available both as hot rolled and cold rolled. Typical applications include bent profiles.

We supply many steel grades according to standards like EN, VDA and different OEM standards. If you don't find a specific standard in the table below, please contact your nearest SSAB representative for more detailed information.

Dimension Range

Hot rolled / UC: thickness 2.00-6.00 mm, width up to 1600 mm.

Slit strip and cut to length sheets are available upon request.

Grade and coating specific restrictions on available dimensions may occur.

Available Standards

VDA 239-100:2016

Docol 500LA

Docol 500LA

USED FOR
STANDARDS
DATA SHEET
USED FOR

Automotive

STANDARDS

VDA239-100:2016

DATA SHEET