GreenCoat Cool acts as a heat shield for your building.

GreenCoat Cool for roofing features special solar heat reflecting properties that make the surface stay cooler than regular coated surfaces. For buildings that need cooling, this product helps to save energy and increases the thermal comfort.

The largest difference in surface temperature between GreenCoat Cool and standard products is achieved for dark colors. 

In the table below you will find typical values for some colors. Total solar reflectance¹ and Thermal IR emittance² describes the product properties. 

The reverse side of the sheet is painted as standard with a two-layer grey backside coating.

SSAB color coated products comply with current REACH regulations and are fully free of chromates. GreenCoat® color coated steels are all manufactured according to EN 10169 + A1.

Podrobnosti o výrobku

Svitky materiálu GreenCoat

Thermal Properties

In the table you will find typical values for some colors. Total solar reflectance¹ and Thermal IR emittance² describes the product properties. 
Dozvědět se další pozornosti

In the table below you will find typical values for some colors. Total solar reflectance¹ and Thermal IR emittance² describes the product properties. 

Thermal total solar reflectance¹ Thermal IR emittance²
Colors GreenCoat Cool Standard color GreenCoat Cool Standard color
015 - Black 0.22 0.05 0.91 0.91
087 - Antracite 0.33 0.10 0.91 0.91
454 - Dark Grey 0.25 0.07 0.91 0.92
859 - Juniper Green 0.27 0.07 0.91 0.92
036 - Lead Grey 0.24 0.08 0.91 0.91
758 - Maroon 0.36 0.23 0.91 0.94

1) Measurements were taken by an accredited independent test laboratory according to ASTM 
2) Measurements were taken by an accredited independent test laboratory according to ASTM EC1371-98

GreenCoat Cool

GreenCoat Cool

USED FOR
MAIN PROPERTIES
COATING
COLOR PALETTE
MATERIÁLOVÝ LIST
USED FOR

Roofing

MAIN PROPERTIES

Energy efficient

Outdoor durability

COATING

Normální

COLOR PALETTE

  • Anthracite Grey
    RR2H8 / SS0087

  • Mountain Grey
    RR23 / SS0036

  • Nordic Night Black
    RR33 / SS0015

  • Acorn Brown
    RR827 / SS0434

  • Cottage Red
    RR29 / SS0758

MATERIÁLOVÝ LIST