    SSAB Domex 500ML is a thermomechanically rolled structural steel plate that provides high strength at low temperatures. SSAB Domex 500ML has no equivalent in any structural standard.

    Dimension Range

    SSAB Domex 500ML is available in thicknesses of 8.00-60.00 mm and in widths up to 3300 mm depending on the thickness. More detailed dimensions are provided in the dimension program.

    Mechanical Properties

    Hide/Show specific columns Edit
    Select columns to display
      Thickness
      (mm)
      Yield strength ReH
      (min MPa)
      Tensile strength Rm
      (MPa)
      Elongation A5
      (min %)
      8.00 - 16.00 500 570 - 760 16
      16.01 - 40.00 480 570 - 760 16
      40.01 - 60.00 470 560 - 760 16
      Compare parameters

      Select one parameter to compare

      Comparison

        The tensile test is made transverse to the rolling direction in compliance with EN 10025-4.

        Impact Properties

        Hide/Show specific columns Edit
        Select columns to display
          Min. impact energy for longitudinal testing,
          Charpy V 10x10 mm test specimens
          40 J / -60 °C
          Compare parameters

          Select one parameter to compare

          Comparison

            Min. impact energy for longitudinal testing,
            Charpy V 10x10 mm test specimens
            40 J / -60 °C

            The impact test is made longitudinally to the rolling direction in compliance with EN 10025-4.

            Chemical Composition (heat analysis)

            Hide/Show specific columns Edit
            Select columns to display
              C
              (max %)
              Si
              (max %)
              Mn
              (max %)
              P
              (max %)
              S
              (max %)
              Al
              (min %)
              Nb
              (max %)
              V
              (max %)
              Ti
              (max %)
              0.18 0.50 1.70 0.020 0.010 0.02 0.05 0.12 0.05
              Compare parameters

              Select one parameter to compare

              Comparison

                Carbon Equivalent

                Hide/Show specific columns Edit
                Select columns to display
                  Thickness (mm) 8.00 - 60.00
                  CET (max ) 0.31
                  CEV (max %) 0.43
                  Compare parameters

                  Select one parameter to compare

                  Comparison

                    Thickness (mm)
                    CET (max )
                    8.00 - 60.00
                    0.31
                    Thickness (mm)
                    CEV (max %)
                    8.00 - 60.00
                    0.43
                    CET and CEV formula

                    Tolerances

                    Thickness

                    SSAB Domex ML products are delivered with tolerances that correspond to ¾ of EN 10029 Class A as default value.

                    Length and Width

                    Width tolerances -0/+4-10 mm depending on the thickness. Length tolerances -0/+15-75 mm depending on length.

                    Shape

                    According to EN 10029.

                    Flatness

                    Maximum flatness deviation 6 mm/m.

                    Surface Properties

                    According to EN 10163-2 Class A, Subclass 3.

                    Delivery Conditions

                    Thermomechanically rolled (M).

                    Fabrication and Other Recommendations

                    Minimum inner bending radius is 1.0 x t transverse to the rolling direction and 1.5 x t longitudinal to the rolling direction up to max 20mm in thickness.

                    For information concerning fabrication, see SSAB´s brochures on www.ssab.com or consult Tech Support.

                    Appropriate health and safety precautions must be taken when bending, welding, cutting, grinding or otherwise working on the products.

                    Contact Information

                    www.ssab.com/contact