    SSAB’s Plastisol P200 is a color coated steel that offers a thick coating and an embossed surface. It combines high wear resistance with high durability against corrosion. P200 is easy to process and can be bent without restrictions.

    The reverse side of the sheet is painted with a two-layer grey backside coating.
     
    P200 complies with current REACH regulations and is fully free of chromates.

    SSAB’s color coated steels are all manufactured according to EN 10169.

    Technical Properties

    Hide/Show specific columns Edit
    Select columns to display
      Technical Properties Embossed
      Gloss n/a
      Minimum inner bending radius 0 x sheet thickness
      Scratch resistance 45 N
      UV radiation resistance RUV2
      Corrosion resistance 1) RC5
      Stain resistance Satisfactory
      Highest operating temperature 60 °C
      Fire classification, EN 13501-1 C- s2 d1
      Coating thickness, nominal (primer + top coat) 200 µm
      Coating structure Embossed
      Steel designation 2) S280GD - S350GD, DX51D
      Zinc coating 275 g/m2
      Min steel thickness 2) 0.42 mm
      Steel width 2) 1000 - 1500 mm
      Compare parameters

      Select one parameter to compare

      Comparison

        Technical Properties
        Gloss
        Embossed
        n/a
        Technical Properties
        Minimum inner bending radius
        Embossed
        0 x sheet thickness
        Technical Properties
        Scratch resistance
        Embossed
        45 N
        Technical Properties
        UV radiation resistance
        Embossed
        RUV2
        Technical Properties
        Corrosion resistance 1)
        Embossed
        RC5
        Technical Properties
        Stain resistance
        Embossed
        Satisfactory
        Technical Properties
        Highest operating temperature
        Embossed
        60 °C
        Technical Properties
        Fire classification, EN 13501-1
        Embossed
        C- s2 d1
        Technical Properties
        Coating thickness, nominal (primer + top coat)
        Embossed
        200 µm
        Technical Properties
        Coating structure
        Embossed
        Embossed
        Technical Properties
        Steel designation 2)
        Embossed
        S280GD - S350GD, DX51D
        Technical Properties
        Zinc coating
        Embossed
        275 g/m2
        Technical Properties
        Min steel thickness 2)
        Embossed
        0.42 mm
        Technical Properties
        Steel width 2)
        Embossed
        1000 - 1500 mm

        1) Classification into corrosion resistance categories is based on blistering, delamination and damage on bend of the coating after two years exposure in natural outdoor testing sites as specified in EN 10169.

        2) Maximum steel thickness is 1.5 mm and maximum steel width depends on steel thickness. For other steel dimensions or steel grades please contact SSAB Tech Support.

        Colors

        Below are the colors currently available. Other colors can be agreed upon separately.

        Colors shown in the color table are only indicative. To see the real visual appearance of the product, please order a color sample. Please note also that the same colors between the products may differ.

        4 Available Colors
        Preview colors
        Close

        Colors

        P200

        White

        RR120 / SS----

        Embossed

        Anthracite Grey

        RR2H8 / SS0087

        Embossed

        Nordic Night Black

        RR33 / SS0015

        Embossed

        Walnut Brown

        RR32 / SS0387

        Embossed

        Reverse Side Coating

        Unless otherwise specified, the reverse side of the sheet is painted with a two-layer coating to further improve the corrosion resistance of the end product. The coating provides good adhesion properties to many adhesives and foams; nevertheless the compatibility needs to be tested case-specifically.

        Hide/Show specific columns Edit
        Select columns to display
          Technical Properties
          Nominal Coating Thickness (primer + top coat) 12 µm
          Color Grey
          Corrosion Resistance Min CPI3
          Compare parameters

          Select one parameter to compare

          Comparison

            Technical Properties
            Nominal Coating Thickness (primer + top coat)
            12 µm
            Technical Properties
            Color
            Grey
            Technical Properties
            Corrosion Resistance
            Min CPI3

            For easy material identification the reverse side of the sheet is stamped with the SSAB logo and the product name. The production year is marked to ease material traceability and can be referred to within the guarantee period. An arrow shows the direction of production to ensure installation in a uniform direction.