GreenCoat Pural

GreenCoat Pural

A specially developed roof product

GreenCoat Pural is a highly durable product for roofing, suitable for standing seam roofs, tiles and profiles.

GreenCoat Pural, available in regular and matt finishes, can also be used in wall panels and protective flashings. The chemical composition of the Pural coating is optimized to resist weathering, resulting in excellent corrosion and UV resistance properties. The slightly textured surface helps protect against mechanical wear. 

GreenCoat Pural is easy to handle during manufacturing.

The reverse side of the sheet is painted as standard with a two-layer grey backside coating. SSAB color coated products comply with current REACH regulations and are fully free of chromates. GreenCoat® color coated steels are all manufactured according to EN 10169 + A1.

Product details

In this section, you will find our Nordic quality steels and zinc coatings that we recommend for use with our wide coating offer. Details about product dimensions are also available.
Learn more

Product details

In this section, you will find our wide product offering with our Nordic quality steels and zinc coatings recommended for different applications. Details about product dimensions are also available.

Main applications  Recommended product*  Recommended steels Recommended Zinc mass Min thickness**  Width range*** 
Roofing, tinsmith
GreenCoat PLX Pro BT PLX Z350 0.60 mm 1000-1500 mm
 GreenCoat FAP Pro BT FAP  Z350  0.60 mm 1000-1500 mm 
GreenCoat PLX Legacy PLX Z350 0.60 mm 1000-1500 mm
           
Roofing, tiles & profiles GreenCoat Pural BT S280GD, S320GD, S350GD
Z275 0.50 mm 1000-1500 mm
GreenCoat Pro BT S280GD, S320GD, S350GD
Z275 0.50 mm 1000-1500 mm
GreenCoat Mica BT S280GD, S320GD, S350GD
Z275 0.50 mm 1000-1500 mm
GreenCoat Crown BT S280GD, S320GD, S350GD
Z275 0.50 mm 1000-1300 mm
Rough Matt Polyester S280GD, S320GD, S350GD
 Z275 0.45 mm  1000-1424 mm
Polyester S280GD-S350GD, DX51D
Z275 0.42 mm 1000-1500 mm
           
Roofing, modular GreenCoat Crown BT S280GD, S320GD, S350GD Z275 0.50 mm 1000-1300 mm
           
Rain water systems GreenCoat RWS FAX, PLX Z275 0.50 mm 1000-1500 mm
           
Facades GreenCoat Hiarc S280GD, S320GD, DX51D 
Z275 0.50 mm 1000-1500 mm
GreenCoat Hiarc Max S280GD, S320GD, DX51D 
Z275 0.50 mm 1000-1500 mm
GreenCoat Hiarc Cool S280GD, S320GD, DX51D 
Z275 0.50 mm 1000-1500 mm 
GreenCoat Anti-Graffiti BT S280GD, S320GD, DX51D 
Z275 0.50 mm 1000-1500 mm
GreenCoat Crown BT S280GD, S320GD
Z275 0.50 mm 1000-1300 mm
Polyester S280GD, S320GD, DX51D 
Z275 0.42 mm 1000-1500 mm
           
Indoor applications Polyester Indoor S250GD-S350GD, DX51D 
Z100 0.40 mm 1000-1424 mm
GreenCoat Foodsafe BT S250GD-S350GD, DX51D 
Z100 0.50 mm 1000-1500 mm
Laminate Foodsafe S250GD-S350GD, DX51D 
Z275 0.42 mm 1000-1400 mm
Epoxy S250GD-S350GD, DX51D 
Z100 0.40 mm 1000-1500 mm

* In addition to these we have a wide range of so called custom made products. Please contact SSAB Europe Tech support.
** Please take into account the country specific building recommendations concerning the minimum thickness. If other thicknesses are required, please contact SSAB Tech Support. Max thickness is 1,5 mm.
*** Max width depends on steel thickness. If other steel dimensions are needed, please contact SSAB Tech Support.

GreenCoat coils

USED FOR
MAIN PROPERTIES
COATING
COLOR PALETTE