St. Paul

SSAB North American Division
2500 West County Road B
Roseville, Minnesota 55113-3873

Toll Free:  800-383-9031
Tel:  651-631-9031
Fax:  651-631-9670

Works Manager:  Joseph Folio


Products

  • Temper leveled cut-to-length sheet and plate
  • 0.100" through 0.500" thick
  • 48" through 96" wide
  • 48" through 720" lengths
  • Up to 0.500" x 96" at 100,000 psi yield strength
  • Flatness tolerances of ½ ASTM for all grades and ¼ ASTM for a wide range of product sizes
Principal Equipment

Annual Capacity (Tons)

21" diameter work roll
45" diameter back-up roll
Work roll bending

300,000

0.500" x 96" cut-to-length line 


Certificate

 QMI