Coil Processing

SSAB, a global niche producer of high strength steel with a leading market position and productivity, develops solutions in order to increase the competitiveness of its customers.

SSAB North American Division (NAD) operates cut-to-length equipment in Surrey, British Columbia, Toronto, Ontario, St. Paul, Minnesota, and Houston, Texas. The cut-to-length facilities in Toronto, St. Paul, and Houston feature state-of-the-art temper mills and cut-to-length lines. NAD processes steel coils of various widths, gauges and grades, cutting them to specific lengths to meet customer requirements.

SSAB North American Division's customers include Service Centres, who purchase processed material for re-sale, Fabricators, OEM's (Original Equipment Manufacturers) and Job Shops, who further process the steel.

Major Product Groups

SSAB North American Division facilities have the capability to flatten, level, and cut coiled steel to specified lengths. These lengths range from pieces as short as 2' in length to over 60'. NAD produces a wide range of products in yields as high as 100,000 psi, thicknesses up to 1/2" and widths as wide as 96". NAD's current lines meet 1/2 commercial tolerance values on all disciplines associated with grading the product.

Temper Leveled Products

SSAB North American Division's Toronto, St. Paul, and Houston Works feature Temper Levelled Cut-To-Length lines that are able to meet 1/4 tolerance on a wide range of product sizes.

The premium finished quality of Temper Leveled Coil (TLC) results in improved performance and total cycle savings through increased productivity and lower finished product rejection rates. The consistency of the product contributes to increased savings through reduced set up costs.

 With conventional leveling the external surface of the plate or sheet appears flat, but the core retains its coiled memory. Fabrication processes will release this memory, causing distortion.

SSAB North American Division’s TLC process has solved this problem. The process erases coil memory throughout the plate - eliminating cross-break, cross-bow and edge wave. Whether you Punch, Form or Burn, products remain flat throughout the manufacturing process.

Another aspect of the TLC process is Total Lower Cost, one of its greatest advantages. Consider the savings realized through:

  • J.I.T. deliveries
  • Exact lengths on short notice
  • Cut-to-length deliveries versus mill deliveries
  • Reduced costs of inventory possession
  • Elimination of tip-ups due to coil memory when burning
  • Reduced time in surface preparation resulting in a surface finish that is superior to cross rolled discrete plate

When leveling without tension, only the surface of the material is stretched beyond its yield point. Leveling with tension and compression means the full 100% of the material cross section is stretched beyond its yield point.

NAD's TLC temper mills provide assurance that the plate from the coil remains perfectly flat.

TLC Camber Tolerances
Length

Mill Edge

Cut Edge

96" to 120"

1/8"

1/16"

over 120" to 240"

3/16"

3/32"

over 240" to 720"

1/4"

1/8"

 

TLC Length Tolerances
Length

Up To 0.250"

Over 0.251"

up to 120"

± 1/32"

± 1/16"

over 120" to 240"

N/A

± 1/16"

over 240" to 360"

N/A

± 1/8"

over 360" to 720"

N/A

± 1/4"

 

TLC Flatness Tolerances Through 50 ksi
Gauge

48"- 59"

60"- 71"

72"- 83"

84"- 95"

96"

0.188" - 0.249"

3/16

5/16

5/16

3/8

3/8

0.250" - 0.374"

3/16

3/16

1/4

5/16

5/16

0.375" - 0.499"

1/8

1/8

3/16

3/16

1/4

0.500" - 0.750"

1/8

1/8

1/8

3/16

1/4

 

Standard GradesHigh Strength Special Grades

CSA
G40.21 300W
G40.21 350W
G40.21 400W

AISI/SAE
1008 to 1020

ASTM
A36
A569
A570
A572
A607
A656
A709
A715

CSA
G40.21 350A
G40.21 350AT
G40.21 350WT

AISI/SAE
J410 950XK
4130
5150
8620

ASTM
A242 Type 1
A516 GR70
A572 GR65
A606 Type 4
A607 GR60
A656 GR80
A715 GR70
A871 GR65
Other
AR200
ABS-A
Cu - Bearing
Customer Specs
TLC

Major End Uses

  • Construction
  • Grain Bins
  • Oil/Gas Storage Tanks
  • Various parts of Agricultural Equipment
  • Truck Frames and Boxes
  • Railway Car Components
  • Yard and Garden Care Equipment (Mowers, Tillers, etc.)
  • Bus Components
  • Power Pole Components
  • Bridges