| Statistics (ktonnes unless otherwise stated) | 2002 | 2003 | 2004 | 2005 | 2006 |
| | | | | | |
| Production of crude steel in the group | 3 881 | 3 911 | 4 142 | 3 966 | 3 737 |
| Production of slabs in the group | 3 661 | 3 620 | 3 834 | 3 642 | 3 413 |
| Production of hot rolled steel sheet and plate | 3 257 | 3 286 | 3 284 | 3 072 | 3 246 |
| - Strip Products Division | 2 675 | 2 640 | 2 633 | 2 440 | 2 660 |
| - Plate Division | 582 | 646 | 651 | 632 | 586 |
| | | | | | |
| Shipments in the Steel Operation | 3 113 | 3 130 | 3 187 | 2 972 | 3 096 |
| - Strip Products Division | 2 538 | 2 480 | 2 492 | 2 311 | 2 474 |
| - Plate Division | 575 | 650 | 695 | 661 | 622 |
| | | | | | |
| Shipments of core niche products | 594 | 697 | 893 | 978 | 1 209 |
| - EHS/UHS | 278 | 331 | 447 | 507 | 699 |
| - Quenched & Tempered heavy plate | 316 | 366 | 447 | 471 | 510 |
| | | | | | |
| Core niche products as % of total shipments in the steel operation | 19 | 22 | 28 | 33 | 39 |
| EHS/UHS as % of total steel sheet shipments | 11 | 13 | 18 | 22 | 28 |
| Quenched & tempered heavy plate as % of total plate shipments | 55 | 56 | 64 | 71 | 82 |
| | | | | | |
| Statistics (ktonnes unless otherwise stated) | 1Q06 | 2Q06 | 3Q06 | 4Q06 | 1Q07 | 2Q07 | 3Q07 |
| | | | | | | |
| Production of crude steel in the group | 1024 | 991 | 778 | 943 | 1039 | 1030 | 855 |
| Production of slabs in the group | 945 | 901 | 710 | 857 | 940 | 943 | 780 |
| Production of hot rolled steel sheet and plate | 866 | 891 | 659 | 830 | 876 | 832 | 671 |
| - Strip Products Division | 710 | 733 | 539 | 678 | 727 | 686 | 548 |
| - Plate Division | 156 | 158 | 120 | 152 | 149 | 146 | 123 |
| | | | | | | |
| Shipments in the Steel Operation | 815 | 841 | 652 | 788 | 830 | 807 | 667 |
| - Strip Products Division | 646 | 679 | 525 | 624 | 665 | 656 | 530 |
| - Plate Division | 169 | 162 | 127 | 164 | 165 | 151 | 137 |
| | | | | | | |
| Shipments of core niche products | 305 | 328 | 265 | 313 | 357 | 350 | 318 |
| - AHSS | 170 | 195 | 154 | 180 | 212 | 213 | 189 |
| - Quenched & Tempered heavy plate | 135 | 132 | 111 | 133 | 145 | 137 | 129 |
| | | | | | | |
| Core niche products as % of total shipments in the steel operation | 37 | 39 | 41 | 40 | 43 | 43 | 48 |
| EHS/UHS as % of total steel sheet shipments | 26 | 29 | 29 | 29 | 32 | 32 | 36 |
| Quenched & tempered heavy plate as % of total plate shipments | 80 | 81 | 87 | 81 | 88 | 91 | 94 |