Product/grade Example of application Fact sheets
Overlay Products
Chromium carbide overlay plate Chromium Carbide Overlay Plate Datasheet
Laser Quality Plate
Laser quality plate Multiple Laser Quality
As-Rolled Plate Products
Structural steel Bridges Structural Steel - Bridges
CSA Structural Steel - Bridges Bridges CSA Structural Steel - Bridges
API 2MT1  Cold forming and welding API 2MT1
API 2W-50 Cold forming and welding API 2W-50
AR200 Cement mixer drums and fins, bulk material handling chute liners, skirtboard liners, and screw conveyers
AR200
A656 Grade 80  Truck frames, transport trailers, construction equipment, agriculture equipment, crane booms, mobile manlifts, and rail cars A656 Grade 80
ST 100F TL Transport trailers, construction equipment, crane booms, mobile manlifts, agricultural equipment, heavy vehicle frames, and chassis. ST 100XF TL
A829-4140 Variety of mold, tool and die applications A829-4140
Normalized Plate Products
A516 Welded pressure vessels A516
2H - 50 Offshore structures 2H - 50
A633 Grade E Utility pole base plates, jack up rig legs for offshore platforms, booms, car bodies, crawler frames, electric shovel dipper handles, and suspension components A633 Grade E
Q&T Plate Products
A514 Grade B Transport trailers, construction equipment, crane booms, mobile man-lifts, agricultural equipment, heavy vehicle frames and chassis, and welded bridge structural members. A514 Grade B
A514 Grade S Transport trailers, construction equipment, crane booms, mobile man-lifts, agricultural equipment, heavy vehicle frames and chassis, and welded bridge structural members A514 Grade S
AR400F Truck beds, buckets, hoppers, chutes, crushers, conveyor troughs, bulldozers, excavators, and concrete mixer drums AR400F
AR450F Hoppers, chutes, crushers, conveyors, screens, shovels and buckets, cutting edges, truck dump bodies, and other components exposed to abrasive wear. AR450F
AR500F Hoppers, chutes, crushers, conveyors, screens, shovels and buckets, cutting edges, truck dump bodies, and other components exposed to abrasive wear. AR500F