Docol - Mild Steels

New designation Former designation
EN 10027-1
and ECISS IC10
EN 10027-2 EN 10130 Sweden
SS
14 xxx
Germany
DIN-T1
1623
Great Br.
BS
1449-1
France
NF A
36-401
Finland
SFS
600
Italy
UNI
5866
Spain
UNE
36086
USA Japan
DC01 1.0330 FeP01 1142 St 12 CR 4 C CR 2 Fe P01 AP 00 A 366 SPCD
DC03 1.0347 FeP03 1146 St 13 CR 3 CR 2 E CR 3 Fe P02 AP 02 A 619 SPCE
DC04 1.0338 FeP04 1147 St 14 CR 1 ES CR 4 Fe P04 AP 04 A 620 SPCEN
DC05 1.0312 FeP05 - St 14 - - - - - - -
DC06 1.0873 FeP06 - - - - - - - - -
Docol 4D - - - - - - - - - - -


Docol - High Strength Steels

SSAB Tunnplat
Steel grade
SS
14xxx
BS
1449
SEW
093

094

NF A36-203

EN 10268

EN 10155
Docol 220 RP - - - ZStE 220 P - - -
Docol 260 RP - - ZStE 260 P - - -
Docol 300 RP - - - ZStE 300 P - - -
Docol 220 BH - - - ZStE 220 BH - - -
Docol 260 BH - - - ZStE 260 BH - - -
Docol 300 BH - - - ZStE 300 BH - - -
Docol 220 YP 1316 CR37/23 - - - - -
Docol 240 LA - - - - - H 240 LA -
Docol 260 YP - - ZStE 260 - - - -
Docol 280 YP 1426 - - - E 275 D - -
Docol 280 LA - - - - - H 280 LA -
Docol 300 YP - CR40/30 ZStE 300 - - - -
Docol 320 LA - - - - - H320 LA -
Docol 340 YP - - ZStE 340 - E 335 D - -
Docol 350 YP 2136 CR43/35 - - - - -
Docol 360 LA - - - - - H360 LA -
Docol 380 YP - - ZStE 380 - - - -
Docol 400 LA - - - - - H 400 LA -
Docol 420 YP - - ZStE 420 - E 430 D - -
Docol 500 YP - - - - E 490 D - -
Docol 355 W - - - - - - JOWP