In Steelfacts you will find the most relevant mechanical properties and manufacturing recommendations. It is the perfect tool at the initial stage of material choice for a component and as input for FE-simulations. The data can be accessed by specifying the SSAB steel grade or by specifying the relevant asked for mechanical properties. Among the content can be mentioned;
- Structural mechanical properties (typical stress-strain curves)
- Forming recommendations and properties (minimum recommended bending radius, flanging recommendations, Forming Limit Diagrams (FLD) etc)
- Welding recommendations (welding consumables, process parameters etc)
If you do not find the asked for information, please contact .
The information on Steelfacts is valid at the date of publication and is subject to change without prior notice, as a result of on-going process and product development.