Boron grades are manufactured to EN 10083-3. With carbon contents up to 0.20% and low aluminium content. Case hardening steels are manufactured according to EN 10084. Hardenable steels are available with thicknesses between 2.00mm and 10.00mm and a maximum width of 1600mm, grade dependant. Material is supplied with "as rolled" properties and hardness/strength is developed by conventional heat treatment. Typical applications include agricultural parts, washers, knives and gear wheels. As these steels are supplied with "as rolled properties", all normal fabrication methods can be used without difficulty. Welding may be carried out using all standard methods. Further information is available on request.