Dogal is available up to min 1000 N/mm² tensile strength. The surface has a uniform appearance which provides a good substrate for painting. Dogal is used for products that need protection against corrosion, such as washing machines, fans and ventilation ducts.

Dogal is also used in the automotive industry, where its high strength and good workability are put to use.