Docol - Aceros suaves
| Nueva designación |
Designación anterior |
EN 10027-1 y ECISS IC10 |
EN 10027-2 |
EN 10130 |
Suecia SS 14 xxx |
Alemania DIN-T1 1623 |
Reino Unido BS 1449-1 |
Francia NF A 36-401 |
Finlandia SFS 600 |
Italia UNI 5866 |
España UNE 36086 |
EE.UU. |
Japón |
| DC01 |
1.0330 |
FeP01 |
1142 |
St 12 |
CR 4 |
C |
CR 2 |
Fe P01 |
AP 00 |
A 366 |
SPCD |
| DC03 |
1.0347 |
FeP03 |
1146 |
St 13 |
CR 3 CR 2 |
E |
CR 3 |
Fe P02 |
AP 02 |
A 619 |
SPCE |
| DC04 |
1.0338 |
FeP04 |
1147 |
St 14 |
CR 1 |
ES |
CR 4 |
Fe P04 |
AP 04 |
A 620 |
SPCEN |
| DC05 |
1.0312 |
FeP05 |
- |
St 14 |
- |
- |
- |
- |
- |
- |
- |
| DC06 |
1.0873 |
FeP06 |
- |
- |
- |
- |
- |
- |
- |
- |
- |
| Docol 4D |
- |
- |
- |
- |
- |
- |
- |
- |
- |
- |
- |
Docol - Aceros de alta resistencia
SSAB Tunnplat Calidad de acero |
SS 14xxx |
BS 1449 |
SEW 093 |
094 |
NF A36-203 |
EN 10268 |
EN 10155 |
| Docol 220 RP |
- |
- |
- |
ZStE 220 P |
- |
- |
- |
| Docol 260 RP |
- |
- |
- |
ZStE 260 P |
- |
- |
- |
| Docol 300 RP |
- |
- |
- |
ZStE 300 P |
- |
- |
- |
| Docol 220 BH |
- |
- |
- |
ZStE 220 BH |
- |
- |
- |
| Docol 260 BH |
- |
- |
- |
ZStE 260 BH |
- |
- |
- |
| Docol 300 BH |
- |
- |
- |
ZStE 300 BH |
- |
- |
- |
| Docol 220 YP |
1316 |
CR37/23 |
- |
- |
- |
- |
- |
| Docol 240 LA |
- |
- |
- |
- |
- |
H 240 LA |
- |
| Docol 260 YP |
- |
- |
ZStE 260 |
- |
- |
- |
- |
| Docol 280 YP |
1426 |
- |
- |
- |
E 275 D |
- |
- |
| Docol 280 LA |
- |
- |
- |
- |
- |
H 280 LA |
- |
| Docol 300 YP |
- |
CR40/30 |
ZStE 300 |
- |
- |
- |
- |
| Docol 320 LA |
- |
- |
- |
- |
- |
H320 LA |
- |
| Docol 340 YP |
- |
- |
ZStE 340 |
- |
E 335 D |
- |
- |
| Docol 350 YP |
2136 |
CR43/35 |
- |
- |
- |
- |
- |
| Docol 360 LA |
- |
- |
- |
- |
- |
H360 LA |
- |
| Docol 380 YP |
- |
- |
ZStE 380 |
- |
- |
- |
- |
| Docol 400 LA |
- |
- |
- |
- |
- |
H 400 LA |
- |
| Docol 420 YP |
- |
- |
ZStE 420 |
- |
E 430 D |
- |
- |
| Docol 500 YP |
- |
- |
- |
- |
E 490 D |
- |
- |
| Docol 355 W |
- |
- |
- |
- |
- |
- |
JOWP |