Domex 960
Domex 960 is a thermomechanical rolled ultra high strength steel with minimum yield strength of 960 MPa
|
|
|
|
Domex Wear 400
Domex Wear 400 is a quenced wear resistant steel suited for applications subject to abrasion where demands on high material strength and impact toughness are essential.
|
|
- Pipes for grain
- Conveyers
- Truck bodies
- Feeders
- Loader buckets
- Concrete mixers
- Timber grapples
|
|
Domex 700 MC
Domex MC is a range of high strength cold-forming steels distinguished by high strength, excellent form-ability and good weldability, which makes them suitable for a wide range of applications
|
|
- Truck chassis
- Cranes
- Earthmoving machines
|
|
Domex 650 MC
Domex MC is a range of high strength cold-forming steels distinguished by high strength, excellent form-ability and good weldability, which makes them suitable for a wide range of applications
|
|
- Truck chassis
- Cranes
- Earthmoving machines
|
|
Domex 640 XP
|
|
|
|
Domex 600 MC
Domex MC is a range of high strength cold-forming steels distinguished by high strength, excellent form-ability and good weldability, which makes them suitable for a wide range of applications
|
|
- Truck chassis
- Cranes
- Earthmoving machines
|
|
Domex 590 XP
|
|
|
|
Domex 550 MC
Domex MC is a range of high strength cold-forming steels distinguished by high strength, excellent form-ability and good weldability, which makes them suitable for a wide range of applications
|
|
- Truck chassis
- Cranes
- Earthmoving machines
|
|
Domex 500 MC
Domex MC is a range of high strength cold-forming steels distinguished by high strength, excellent form-ability and good weldability, which makes them suitable for a wide range of applications
|
|
- Truck chassis
- Cranes
- Earthmoving machines
|
|
Domex 460 MC
Domex MC is a range of high strength cold-forming steels distinguished by high strength, excellent form-ability and good weldability, which makes them suitable for a wide range of applications
|
|
- Truck chassis
- Cranes
- Earthmoving machines
|
|
Domex 460 XPE/Domex 420 MCE
Domex MC is a range of high strength cold-forming steels distinguished by high strength, excellent form-ability and good weldability, which makes them suitable for a wide range of applications
|
|
|
|
Domex 420 MC
Domex MC is a range of high strength cold-forming steels distinguished by high strength, excellent form-ability and good weldability, which makes them suitable for a wide range of applications
|
|
- Truck chassis
- Cranes
- Earthmoving machines
|
|
Domex 420 MC D
Domex MC is a range of high strength cold-forming steels distinguished by high strength, excellent form-ability and good weldability, which makes them suitable for a wide range of applications
|
|
|
|
Domex 355 MC
Domex MC is a range of high strength cold-forming steels distinguished by high strength, excellent form-ability and good weldability, which makes them suitable for a wide range of applications
|
|
- Truck chassis
- Cranes
- Earthmoving machines
|
|
Domex 315 MC
Domex MC is a range of high strength cold-forming steels distinguished by high strength, excellent form-ability and good weldability, which makes them suitable for a wide range of applications
|
|
- Truck chassis
- Cranes
- Earthmoving machines
|
|
Domex 700 W
Domex 350 W and 550 W are high strength and extra high strength respectively, corrosion resistant steels. They are characterised by good formability, impact toughness and weldability. Corrosion resistance is imparted by the formation of a dense, uniform oxide layer after a couple of years in-situ
|
|
- Vehicle chassis
- Container frames
- Bridges buildings
- Chimneys
- Rail wagons
- Snow sheds
- Different kinds of masts
|
|
Domex 550 W
Domex 350 W and 550 W are high strength and extra high strength respectively, corrosion resistant steels. They are characterised by good formability, impact toughness and weldability. Corrosion resistance is imparted by the formation of a dense, uniform oxide layer after a couple of years in-situ
|
|
- Vehicle underbodies
- Container frame structures
- Bridges and building construcions
- Chimney cases
- Rail wagons
- Snow sheds
- Different kinds of masts
|
|
High Carbon Steel
The Domex range of hardenable steels comprises plain carbon and alloyed carbon steels together with a range of Boron alloyed qualities. Carbon steels are available to EN 10083-1.
|
|
- Spades
- Knives
- Saw blades
- Caterpillar tracks
|
|
Boron Steels
The Domex range of hardenable steels comprises plain carbon and alloyed carbon steels together with a range of Boron alloyed qualities. Boron grades are manufactured to EN 10083-3.
|
|
- Spades
- Knives
- Saw blades
- Caterpillar tracks
|
|
Domex 240 YP
Domex MC is a range of high strength cold-forming steels distinguished by high strength, excellent form-ability and good weldability, which makes them suitable for a wide range of applications
|
|
|
|
Domex 200
Domex 200 is an hot rolled steel with excellent forming properties
|
|
- Mountings
- Brackets
- Beams
- Chassis members
- Wheels
- Brake cylinders
- Ball-bearing
- Cages and fans
|
|