| Steel grade |
MMA |
MIG/MAG Solid wire |
MIG/MAG Tubular wire |
SAW |
Domex 220-420 YP Domex 280-420 XP Domex 315-460 MC |
AWS: A5.1 E7X18 DIN 1913: E5153810 EN- 499: E42XX-xx |
AWS: A5.18 ER7XS-X DIN 8559: SG2 EN-440: G42X-xx
|
AWS: A5.20 E7XT-X DIN8558: T521 EN- 758: T42X-xx |
AWS: A5.23/ F7AX-EM12K |
Domex 490 XP Domex 500 MC |
AWS: A5.5 E8X18 DIN 8529: EY5543MnMoB EN- 499: E50X-xx |
AWS: A5.28 ER 8XS-X DIN 8559: SG2 EN-440: G50X-xx |
AWS: A5.29 E8XT-X DIN7084: 541 EN- 758: T50X-xx |
AWS: A5.23/F8AX-EX |
Domex 590 XP Domex 550-600 MC |
AWS: A5.5 E10X18 DIN 8529: EY 69565Mn2NiCrMoB EN- 757: E62X-xx |
AWS: A5.28: ER10XS-X |
AWS: A5.29 E10XT-X |
AWS: A5.23/F10A4-EX |
Domex 640-690 XP Domex 650 MC |
AWS: A5.5 E11X18 DIN 8529: EY 69565Mn2NiCrMoB EN -E757: E69X-xx |
AWS: A5.28: ER10XS-X AWS: A5.28: ER11XS-X DIN SGNiMoCr2 |
AWS: A5.29 E11XT-X |
AWS: A5.23/F11A4-EX |
Domex 740 XP Domex 700 MC |
AWS: A5.5 E12X18 DIN 8529: EY 69565Mn2NiCrMoB EN -E757: E79X-xx |
AWS: A5.28 ER11XS-X AWS: A5.28 ER12XS-X DIN SGNiMoCr2 |
AWS: A5.29 E11XT-X AWS: A5.29 E12XT-X |
AWS: A5.23/F11A4-EX |
| Domex Wear |
AWS: A5.1 E7X18 DIN 1913: E5153810 EN- 499: E42XX-xx |
AWS: A5.18 ER7XS-X DIN 8559: SG2 EN-440: G42X-xx |
AWS: A5.20 E7XT-X DIN8558: T52X-xx EN- 758: T42X-xx |
AWS: A5.23 EM12X/F7AZ-EX EN-756: S42 |
| Domex 355W |
AWS: A5.5 E7X18 DIN 1913: E5155 EN-499: EN46X-xx |
AWS: A5.28 ER8XS-X |
AWS: A5.29 E7XT-X EN-758: T50X-xx |
|
| Domex 014-044 Bor |
AWS: A5.1 E7X18 EN- 499:542XX-xx AWS: A5.5 E12X18 EN -E757: E79X-xx |
AWS: A5.18 ER70S-X EN-440: G42X-xx AWS:A5.28 ER12XS-X |
AWS: A5.20 E7XT-X EN- 758: T42X-xx AWS:A5.29 E12XT-X |
Before hardening
After hardening |
| |
|
|
|
|
DC 01- DC06 Docol 220-420 YP Docol 400-500 DP Docol 220-300 RP Docol 220-300 BH |
AWS: A5.1 E7X18 DIN 1913: E5153810 EN- 499: E42XX-xx |
AWS: A5.18 ER7XS-X DIN 8559: SG2 EN-440: G42X-xx |
|
|
Docol 500 YP Docol 600 DL Docol 600 DP |
AWS: A5.5 E8X18 DIN 8529: EY5543MnMoB EN- 499: E50X-xx |
AWS: A5.28 ER 8XS-X DIN 8559: SG2 EN-440: G50X-xx |
|
|
Docol 800 DL Docol 800 DP |
AWS: A5.5 E11X18 DIN 8529: EY 69565Mn2NiCrMoB EN -E757: E69X-xx |
AWS: A5.28: ER10XS-X AWS: A5.28: ER11XS-X DIN SGNiMoCr2 |
|
|
| Docol 1000-1400 DP |
AWS: A5.5 E12X18 DIN 8529: EY 69565Mn2NiCrMoB EN -E757: E79X-xx |
AWS: A5.28 ER11XS-X AWS: A5.28 ER12XS-X DIN SGNiMoCr2 |
|
|
| Docol 355W |
AWS: A5.5 E7X18 DIN 1913: E5155 EN-499: EN46X-xx |
AWS: A5.28 ER8XS-X |
|
|
| Docol Bo 02-04 |
AWS: A5.1 E7X18 EN- 499:542XX-xx AWS: A5.5 E12X18 EN -E757: E79X-xx |
AWS: A5.18 ER70S-X EN-440: G42X-xx AWS:A5.28 ER12XS-X |
|
Before hardening
After hardening |
Dogal B500 Dogal F26-F40 Dogal 260-420 YP Dogal 180-260 RP Dogal SUB250-350 |
AWS: A5.1 E7X18 DIN 1913: E5153810 EN- 499: E42XX-xx
|
AWS: A5.18 ER7XS-X DIN 8559: SG2 EN-440: G42X-xx
|
|
|
Dogal 500 YP Dogal 600 DP
|
AWS: A5.5 E8X18 DIN 8529: EY5543MnMoB EN- 499: E50X-xx
|
AWS: A5.28 ER 8XS-X DIN 8559: SG2 EN-440: G50X-xx
|
|
|
| Dogal 800 DP |
AWS: A5.5 E11X18 DIN 8529: EY 69565 Mn2NiCrMoB EN -E757: E69X-xx
|
AWS: A5.28: ER10XS-X AWS: A5.28: ER11XS-X DIN SGNiMoCr2
|
|
|