Strapping Steels- Docol Strap
Docol packaging strap steel is supplied in quenched and tempered condition. These steels replace traditional hardened strap.
Hardenable Steels
Cold-rolled hardenable steels are available as high carbon and case hardening steels. The grades in the Docol hardenable steel group are characterized by good formability and by the fact that the very high strength and hardness are archived by hardening the finished part.